Its rightly said "Beauty doesn't need a cover to look
good". The manufacturing process begins with the right selection of wood, complete
seasoning by kilns, a process to reduce the moisture Levels from 65% to 12%, leaving
no chances for joint opening and disfigurement. We keep a quality control with a
regular check at every step by highly qualified technical staff.
Finger Jointed
timber is available in Teak and Gamari Wood as well as in natural color with thickness
of 15, 18, 32, 45, 70 mm the standard size of 1220mm / 2440 mm (8fts/4fts) is available,
specific size according to individual requirement can also be provided. These days,
where more and more plantation timber is used, the girth of the timber becomes insufficient
for effective use in making furniture and doors. Moreover a dimension also suffers
due to inconsistency in quality and sizes of the timber available. Finger jointing
of timber is result of extensive research in this direction. F.J. Timber by nature
is strong much to the Liking of present day generation.
The process of finger jointing
ensures the removable of cracks and dead knots. This results in quality product
which not only increases the strength and Life of the timber but also provides for
a smoother finish, sanded upto 320 grit. Therefore it is a Carpenter delight. |